Design for Ultimate Strength with a Chopped Glass-Filled Phenolic Composite : Critical Flaw Sensitivity, Residual Stress, Fiber Orientation /
Because they retain strength and stiffness at temperatures as high as 180°C (356°F), injection molded, glass-filled phenolic composites have been used in structural applications. However, the strength of this material as measured with ASTM three-point flexure tests may be as much as 80% higher than...